Mehr lesen
Practical, up-to-date techniques for identifying and eliminating common causes of boiler failure
Filled with more than 200 color images, The Nalco Guide to Boiler Failure Analysis , Second Edition categorizes distinct failure modes that typify nearly all boiler problems and walks you, step by step, through their solutions. Each type of failure is classified according to its location, general description, critical factors, identification, elimination, cautions, and related problems. Real-world case histories are included throughout. This authoritative resource contains new chapters on:
Phosphate corrosion
Stress-assisted corrosion
Steam and condensate damage
Flow-accelerated corrosion
Comprehensive coverage includes:
Water- and steam-formed deposits Short- and long-term overheating Caustic corrosion Low-pH corrosion Hydrogen damage Chelant complexing Oxygen corrosion Corrosion during cleaning Corrosion fatigue cracking Stress corrosion cracking Graphitic corrosion Dealloying Cavitation Erosion Waterwall fireside corrosion High-temperature furnace corrosion Cold-end corrosion Dew point corrosion Fireside corrosion Welding defects
Inhaltsverzeichnis
Section 1: Waterside Corrosion and Damage
Introduction to Boiler and Steam Systems
Section 1.1: Deposit-Related Problems
Chapter 1. Water-Formed and Steam-Formed Deposits
Section 1.2: Overheating
Chapter 2. Short-Term Overheating
Chapter 3. Long-Term Overheating
Section 1.3: Waterside Corrosion
Chapter 4. Caustic Corrosion
Chapter 5. Low-pH Corrosion during Service
Chapter 6. Hydrogen Damage
Chapter 7. Phosphate Corrosion
Chapter 8. Corrosion by Chelating and Complexing Agents
Chapter 9. Oxygen Corrosion
Chapter 10. Corrosion during Cleaning
Chapter 11. Stress-Assisted Corrosion
Section 1.4: Cracking
Chapter 12. Corrosion Fatigue Cracking
Chapter 13. Stress Corrosion Cracking
Section 1.5: Pre- and Postboiler Damage
Chapter 14. Graphitic Corrosion
Chapter 15. Dealloying
Chapter 16. Steam and Condensate System Damage
Section 1.6: Waterside Flow-Related Damage
Chapter 17. Cavitation
Chapter 18. Erosion and Erosion-Corrosion (Water and Steam Sides)
Chapter 19. Flow-Accelerated Corrosion
Section 2: Fireside Corrosion and Damage
Chapter 20. Waterwall (Furnace) Fireside Corrosion
Chapter 21. High-Temperature Fireside Corrosion
Chapter 22. Cold-End Corrosion during Service
Chapter 23. Dew Point Corrosion during Idle Periods
Chapter 24. Fireside Erosion
Section 3: Material Defects
Chapter 25. Welding Defects
Glossary
Bibliography
Index
Über den Autor / die Autorin
During the past century, Nalco Company has grown from a fledgling water treatment business to the leading integrated water treatment and process improvement company in the world. They do this by focusing on our core markets of water treatment and process chemicals and on our corporate strengths - global presence, on-site expertise, and innovative products and services.Nalco's more than 11,000 employees work with more than 70,000 customers in 130 countries in industry, government and institutions to reduce water and energy consumption by solving and preventing problems, protecting the environment, decreasing costs, increasing productivity, improving profitability by reducing customer total costs of operation, and maintaining asset reliability.
Zusammenfassung
Presented by Nalco, the world’s leading water treatment and process improvement company, this is a comprehensive, up-to-date guide to boiler failure—from material defects to corrosion and cracking.